Unreinforced masonry (URM) cavity-wall construction is a form of masonry where two leaves of clay brick masonry are separated by a continuous air cavity and are interconnected using some form of tie system. A brief historical introduction is followed by details of a survey undertaken to determine the prevalence of URM cavity-wall buildings in New Zealand. Following the 2010/2011 Canterbury earthquakes it was observed that URM cavity-walls generally suffered irreparable damage due to a lack of effective wall restraint and deficient cavity-tie connections, combined with weak mortar strength. It was found that the original cavity-ties were typically corroded due to moisture ingress, resulting in decreased lateral loadbearing capacity of the cavity-walls. Using photographic data pertaining to Christchurch URM buildings that were obtained during post-earthquake reconnaissance, 252 cavity-walls were identified and utilised to study typical construction details and seismic performance. The majority (72%, 182) of the observed damage to URM cavity-wall construction was a result of out-of-plane type wall failures. Three types of out-of-plane wall failure were recognised: (1) overturning response, (2) one-way bending, and (3) two-way bending. In-plane damage was less widely observed (28%) and commonly included diagonal shear cracking through mortar bed joints or bricks. The collected data was used to develop an overview of the most commonly-encountered construction details and to identify typical deficiencies in earthquake response that can be addressed via the selection and implementation of appropriate mitigation interventions. http://www.journals.elsevier.com/structures
The connections between walls of unreinforced masonry (URM) buildings and flexible timber diaphragms are critical building components that must perform adequately before desirable earthquake response of URM buildings may be achieved. Field observations made during the initial reconnaissance and the subsequent damage surveys of clay brick URM buildings following the 2010/2011 Canterbury, New Zealand, earthquakes revealed numerous cases where anchor connections joining masonry walls or parapets with roof or floor diaphragms appeared to have failed prematurely. These observations were more frequent for adhesive anchor connections than for through-bolt connections (i.e., anchorages having plates on the exterior facade of the masonry walls). Subsequently, an in-field test program was undertaken in an attempt to evaluate the performance of adhesive anchor connections between unreinforced clay brick URM walls and roof or floor diaphragm. The study consisted of a total of almost 400 anchor tests conducted in eleven existing URM buildings located in Christchurch, Whanganui and Auckland. Specific objectives of the study included the identification of failure modes of adhesive anchors in existing URM walls and the influence of the following variables on anchor load-displacement response: adhesive type, strength of the masonry materials (brick and mortar), anchor embedment depth, anchor rod diameter, overburden level, anchor rod type, quality of installation, and the use of metal mesh sleeves. In addition, the comparative performance of bent anchors (installed at an angle of minimum 22.5° to the perpendicular projection from the wall surface) and anchors positioned horizontally was investigated. Observations on the performance of wall-to-diaphragm connections in the 2010/2011 Canterbury earthquakes, a summary of the performed experimental program and test results, and a proposed pull-out capacity relationship for adhesive anchors installed into multi-leaf clay brick masonry are presented herein. AM - Accepted Manuscript